Poly(ethylene succinate)
CROW logo
Poly(ethylene succinate)
 

NAMES AND IDENTIFIERS OF POLYMER

POLYMER CLASS Polyesters
COMMON NAMES Poly(ethylene succinate)
STRUCTURE BASED NAME Poly(oxyethyleneoxybutanedioyl), Poly(oxyethyleneoxysuccinyl)
ACRONYMS  
CAS # 25569-53-3
CurlySMILES O{-}CCOC(=O)CCC{n+}(=O)
 

IDENTIFIERS OF MONOMER(S)

CAS # 203-740-4, 107-21-1
COMMON NAMES Succinic acid, Ethanediol
SMILES OC(=O)CCC(=O)O.OCCO
Std. InChI 1S/C4H6O4/c5-3(6)1-2-4(7)8/h1-2H2,(H,5,6)(H,7,8).InChI=1S/C2H6O2/c3-1-2-4/h3-4H,1-2H2.
Std. InChIKey KDYFGRWQOYBRFD-UHFFFAOYSA-N.LYCAIKOWRPUZTN-UHFFFAOYSA-N
STRUCTURE
polyester
 

Thermo-Physical Properties: Experimental / Literature Data

PROPERTYUNITVALUE / RANGEPREFERRED
Molar Volume VmmL mol-1   
Density ρg mL-1   
Solubility Parameter δMPa1/2   
Molar Cohesive Energy Ecoh J mol-1    
Glass Transition Temperature Tg K 262 - 272267
Molar Heat Capacity CpJ (mol K)-1   
Entanglement Molecular Weight Meg mol-1
Index of Refraction nnone 1.47 - 1.481.47
 

Thermo-Physical Properties: Calculated Data

PROPERTYUNITVALUE / RANGEPREFERRED
Molecular Weight of Repeat unitg mol-1 144.13
Van-der-Waals Volume VvWmL mol-1 71.3
Molar Volume VmmL mol-1 102 - 110106
Density ρg mL-1 1.31 - 1.411.36
Solubility Parameter δMPa1/2 20.6 - 22.021.4
Molar Cohesive Energy EcohJ mol-1 43400 - 53100 48700
Glass Transition Temperature TgK 248 - 276267
Molar Heat Capacity CpJ (mol K)-1 252 - 263256
Entanglement Molecular Weight Meg mol-1 2190 - 28202430
Index of Refraction nnone 1.47 - 1.501.48

  Last updated: July 29, 2016